Preparation of an α″‐Fe16N2 Magnet via a Ball Milling and Shock ...
WEBJun 1, 2016 · The volume ratio of the α″‐Fe16N2 phase reaches 70% after 60 h of milling with a ball mill rotation speed of 600 rpm in planetary mode. Its saturation magnetization (Ms) is 210 emu g–1 and the coercivity is 854 Oe at room temperature. After ball milling, shock compaction is used to compact the milled powder sample into a bulk magnet.